Steel grades | Deoxidation practice and fine grained elements | Condition of supply and max. thickness |
A – B (Z35) | Si-Al killed | As rolled – 50 mm |
D (Z35) | Si-Al killed, fine grained AI only | Normalising rolling - 75 mm |
| A – B – D (Z35) | Si-Al killed, fine grained Al/Nb/V/Ti or (Al+Nb+V+Ti) | Thermo-Mechanical Rolling / Thermo-Mechanical Rolling + Accelerated Cooling – 50 mm |
A – B – D - E (Z35) | Si-Al killed, fine grained Al/Nb/V/Ti or (Al+Nb+V+Ti) | Thermo-Mechanical Rolling / Thermo-Mechanical Rolling + Accelerated Cooling – 50 mm |
AH32 – AH36 (Z35) | Si-Al killed, fine grained Al only or with Ti | As rolled – 20 mm |
DH32 – DH36 (Z35) | Si-Al killed, fine grained Al only or with Ti | As rolled – 12 mm |
| AH32 – AH36 - DH32 – DH36 (Z35) | Si-Al killed, fine grained Al only or with Ti | Normalising rolling - 75 mm |
AH32 – AH36 - DH32 – DH36 – EH32 – EH36 (Z35) | Si-Al killed, fine grained Al/Nb/V/Ti or (Al+Nb+V+Ti) | Thermo-Mechanical Rolling / Thermo-Mechanical Rolling + Accelerated Cooling – 50 mm |
AH40-DH40-EH40 (Z35) | Si-Al killed, fine grained (Al+Nb+V+Ti) | Thermo-Mechanical Rolling / Thermo-Mechanical Rolling + Accelerated Cooling – 50 mm |