Steel type: (Stainless Steel)
1) ASTM A31 2 Tp 316L - ASTM A249 Tp 3 16L - EN 10217 Part 7 1 .4404
2) ASTM A312 Tp 304L - ASTM A249 Tp 304L - EN10217 Part 7 14307
3) ASTM A312 Tp 316Ti - ASTM A249 Tp 316LTi- EN 1 0217-7 1.4571
4) ASTM A312 Tp 321 - ASTM A249 Tp 321 -EN10217-7 1.4541
5) ASTM A312 Tp 304 – ASTM A249 Tp 304 – EN10217-7 14301
Size Range: O.D. from 10 to 273 mm
W. Thk from 0.80 to 6 mm
Product Making Process: Laser CO2 or FIBER Equipment
1) COHERENT FL-ARM 8-10 kW
2) IPG-TPS 6000
3) IPG- YLS 8000
4) ROFIN SINAR LASER CO2 DC080W and TRUMPF - TRU Laser Cel 1100
According to Manufacturer Procedure
Heat Treatment Condition: Bright Annealing Solution (950 - 1100 °C)
Annealing and Pickling (800 - 1060 °C)
NDE on Welded Seam: Eddy Current in lieu of Hydraulic Test
According to EN ISO 10893-1 2020 and EN ISO 10893-2 2020
Survey Condition: The subject material to be in compliance, in all respects, with the
requirements specified in RINA Rules Part D Ch. 2 Sect. 2 and shall be
tested accordingly.
General conditions for the approval
-The approval is granted on condition that the RINA Rules for the approval, manufacture, testing and certification of materials are complied with in all respects.
-RINA is to be notified of any change of materials, manufacturing process, quality control routines that may affect the validity of this certificate.